Ferrous Oxide and Calcined Kaolin Eutectic

Oxide Analysis Formula Tolerance
FeO 39.20% 1.76
Al2O3 27.80% 1.00
SiO2 33.00% 2.01
Oxide Weight 366.91
Formula Weight 366.91

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

Frit Softening Point 1210C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy