Kaolin 113

Alternate Names: Kaolen 113

Oxide Analysis Formula Tolerance
CaO 0.20% 0.02
MgO 0.07% 0.01
K2O 0.04% -
Na2O 0.09% 0.01
TiO2 0.33% 0.02
Al2O3 21.31% 1.00
SiO2 70.24% 5.59
Fe2O3 0.48% 0.01
LOI 7.24%n/a
SO4 0.52%n/a
Oxide Weight 443.99
Formula Weight 481.35

Notes

Available in run-of-mine, 25mm and 50mm sizes.

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Kaolin 111
Materials Kaolin 151
Materials Kaolin 115
Materials Kaolin 171
Materials Kaolin 143
Materials Kaolin 114
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

Firing Shrinkage 1000C: 7.3% 1100C: 7.5% 1200C: 7.8% 1250C: 7.9%
Water absorption 1000C: 19.3% 1100C: 18.3% 1200C: 17.5% 1250C: 17%

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy