| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.13% | 0.01 | |
| K2O | 2.62% | 0.13 | |
| Na2O | 0.40% | 0.03 | |
| TiO2 | 0.73% | 0.04 | |
| Al2O3 | 22.50% | 1.00 | |
| SiO2 | 67.30% | 5.08 | |
| Fe2O3 | 0.32% | 0.01 | |
| LOI | 6.00% | n/a | |
| Oxide Weight | 426.13 | ||
| Formula Weight | 453.33 | ||
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |