Alternate Names: Georgia Kaolin
Description: Medium plasticity kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.01 | |
| MgO | 0.10% | 0.01 | |
| SiO2 | 45.40% | 2.01 | |
| Fe2O3 | 0.40% | 0.01 | |
| Al2O3 | 38.30% | 1.00 | |
| TiO2 | 1.40% | 0.05 | |
| Na2O | 0.10% | - | |
| LOI | 13.96% | n/a | |
| Oxide Weight | 228.77 | ||
| Formula Weight | 265.89 | ||
Pioneer clay is used in pressing, casting and extruding bodies. Its fires fairly white and provides moderate to good dry strength. Its chemistry is very close to theoretical kaolin.
Pioneer Kaolin has been a standard for many years in the North American ceramic industry and bodies and glazes.
Typical physical properties as per data sheet TD-49R
Particle size, % < 2 microns 55-65
Mean particle size (microns) 1.0-1.2
325 mesh residue, % max .75
pH, 20% solids 4.0-6.5
Strength (dry M.O.R.), psi
-50:50 clay:flint 300-400
Cone 10 (M.O.R.), psi
-50:50 clay:flint 2500-3000
Cone 10 absorption, % 18-20
Moisture, % max 3.0
Color (fired), Cone 8 100% clay
-brightness, % MgO 85.1
-whiteness index 18.8
P.C.E. Cone 34
C.E.C. (meq./100g) 4.5-5.5

This picture has its own page with more detail, click here to see it.
Cone 10R (top) and cone 11 down to 8 oxidation (downward).

This picture has its own page with more detail, click here to see it.
The material is much less dense than most other ceramic materials (that is why these bags are so tall). When moved the powder within becomes unstable and they are prone to falling over.

This picture has its own page with more detail, click here to see it.
To which kaolin can bentonite be added to give it similar plasticity as #6 Tile kaolin while firing to a similar degree of maturity? I evaluated McNamee kaolin, Pioneer kaolin, EP kaolin, Grolleg kaolin and New Zealand halloysite against the #6 Tile (my code number L3883). I mixed each as a 70:30 mix of kaolin and nepheline syenite (to be able to compare their response to vitrification-inducing feldspar). To get adequate plasticity for throwing, I added 2.5 and 5% sodium bentonite. I slurried each of them up in water, making a total of fifteen separate mixes. From each, I made SHAB test bars and threw them on the potter's wheel (to gauge plasticity). In the end, I found that one of these, with 5% added bentonite, is a credible substitute for #6 Tile kaolin.
| Materials |
EP Kaolin
A kaolin that gels slurries (good for suspending glazes). It has two variations: a low and medium plasticity. It fires white for use in porcelain bodies. |
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Wilco-UPF Kaolin
|
| Materials |
McNamee Kaolin
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk