| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 55.38% | 2.20 | |
| Al2O3 | 42.69% | 1.00 | |
| Fe2O3 | 0.33% | - | |
| TiO2 | 0.06% | - | |
| CaO | 0.06% | - | |
| MgO | 0.21% | 0.01 | |
| K2O | 1.15% | 0.03 | |
| Na2O | 0.12% | - | |
| Oxide Weight | 238.93 | ||
| Formula Weight | 238.93 | ||
| Minerals |
Mica
See Muscovite. |
| Minerals |
Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Glossary |
Calcination
Calcining is simply firing a ceramic material to create a powder of new physical properties. Often it is done to kill the plasticity or burn away the hydrates, carbonates, sulfates of a clay or refractory material. |