Alternate Names: Kuvars 761
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.08% | 0.06 | |
| K2O | 0.16% | 0.07 | |
| Na2O | 0.27% | 0.18 | |
| Al2O3 | 2.41% | 1.00 | |
| SiO2 | 96.90% | 68.24 | |
| LOI | 0.18% | n/a | |
| Oxide Weight | 4,224.75 | ||
| Formula Weight | 4,232.37 | ||
Available in -100, -63 and -45 micron sizes.