Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.06% | - | |
| K2O | 0.18% | 0.01 | |
| TiO2 | 1.50% | 0.05 | |
| Al2O3 | 38.40% | 1.00 | |
| SiO2 | 45.60% | 2.02 | |
| Fe2O3 | 0.40% | 0.01 | |
| LOI | 13.82% | n/a | |
| Oxide Weight | 228.81 | ||
| Formula Weight | 265.50 | ||
Wilklay SA-1 is a high quality, finely pulverized, airfloat kaolin clay filler with properties specifically selected for the coatings, adhesives, rubber, and other industries. It features low viscosities in aqeous systems and performs as a soft clay in rubber compounds. It is an alternative to Pioneer kaolin.
Specific Gravity: 2.6
Moisture, Max% as produced: 1.0
325 mesh residue, Max: 1.0
GE Brightness, % average: 79.5
pH (28% solids), average: 5.4
Oil Absorption, g/100g clay: 32
Viscosity, 62% solids, cps*, max: 400
Raw Color: Cream
Particle size:
% Finer than 20 microns: 97
10 microns: 91
5 microns: 80
2 microns: 60
1 micron: 47
0.5 microns: 35
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |