Alternate Names: Kaolen 151
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.26% | 0.01 | |
| MgO | 0.17% | 0.01 | |
| K2O | 0.13% | - | |
| Na2O | 0.06% | - | |
| TiO2 | 0.22% | 0.01 | |
| Al2O3 | 35.75% | 1.00 | |
| SiO2 | 45.31% | 2.15 | |
| Fe2O3 | 0.75% | 0.01 | |
| LOI | 16.42% | n/a | |
| SO4 | 0.34% | n/a | |
| Oxide Weight | 235.81 | ||
| Formula Weight | 283.29 | ||
Available in minus 20cm, -100 microns, -75 microns.
| Materials |
Kaolin 115
|
| Materials |
Kaolin 171
|
| Materials |
Kaolin 111
|
| Materials |
Kaolin 113
|
| Materials |
Kaolin 114
|
| Materials |
Kaolin 143
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |