| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.03% | - | |
| K2O | 3.65% | 0.11 | |
| MgO | 0.15% | 0.01 | |
| Na2O | 0.08% | - | |
| TiO2 | 0.21% | 0.01 | |
| Al2O3 | 36.17% | 1.00 | |
| SiO2 | 58.22% | 2.73 | |
| Fe2O3 | 1.47% | 0.03 | |
| Oxide Weight | 281.95 | ||
| Formula Weight | 281.95 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |