Alternate Names: DB-Float
Description: American Kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 38.50% | 1.00 | |
| SiO2 | 45.70% | 2.01 | |
| Fe2O3 | 0.40% | 0.01 | |
| TiO2 | 1.40% | 0.05 | |
| CaO | 0.20% | 0.01 | |
| MgO | 0.10% | 0.01 | |
| Na2O | 0.04% | - | |
| K2O | 0.10% | - | |
| SO4 | 12.50% | n/a | |
| Oxide Weight | 229.01 | ||
| Formula Weight | 261.73 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |