Alternate Names: Kuvars 741
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.08% | 0.27 | |
| MgO | 0.08% | 0.38 | |
| K2O | 0.04% | 0.08 | |
| Na2O | 0.09% | 0.27 | |
| TiO2 | 0.03% | 0.07 | |
| Al2O3 | 0.30% | 0.56 | |
| SiO2 | 99.20% | 312.17 | |
| Fe2O3 | 0.04% | 0.05 | |
| LOI | 0.14% | n/a | |
| Oxide Weight | 18,886.49 | ||
| Formula Weight | 18,912.97 | ||
Available in -100, -63 and -45 micron sizes.
| Materials |
Quartz 761
|
| Materials |
Quartz 762
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |