3DP | BSG | AIF | ABR | | BIN | ADV | AGT | PHY | ASR | ALM | uAz | ALS | E11 | JWK | ART | ARC | EBA | LAG | PBA | BLC | NFi | mQi | BIN | 62N | BIO | BSQ | CHP | BDT | BGD | BGP | BFR | Csu | DZc | BRK | HWi | SCS | MCB | SCB | ECS | CSP | OLC | CRE | CPM | CRS | STN | CST | LBS | TIL | C3D | CBM | CLM | ECM | CLO | SLR | CRT | CCT | CLT | GBG | CCO | CCN | CRP | d3S | CGS | OCS | DEC | DFT | TM2 | | Dux | DRP | DSP | ELE | ELT | SEU | MUE | EEE | MEQ | SCE | EQD | EQP | EQM | EMR | SER | EQS | | ETC | P3D | PAR | PAU | PCA | PBF | PDE | PGL | PKB | PMM | PPO | PPP | PSH | PWT | EXT | FEL | TAA | FRC | 9h6 | FLB | kK5 | FLS | FRT | MFM | YtL | F3D | EGK | GNM | DGE | GBC | GBS | GLS | GLI | GLC | GLM | GLR | GLT | MGL | FGE | GLZ | GEQ | EHE | HMT | h79 | HTR | CHS | Niv | I3D | ICS | IDP | IGR | EAP | ISO | Qno | qhK | KAO | KCD | EKB | KIL | MKL | SKL | LNS | LAB | vLv | FRL | 7hb | LEM | CQL | LTR | MSH | MOF | MAN | | MRK | MDS | MMC | MPC | MTS | MTT | | MAM | MAA | MDE | MTE | EMP | MPE | CLM | DEN | PWH | MAT | e38 | MTR | BDW | PMF | MIN | 3MM | MMK | EMM | MNC | EMF | yPu | NOX | SOC | | DSL | OPA | QKk | OXI | RED | PTT | SWS | PPS | PRP | | SPM | MPB | SPB | FRP | 9Hv | POI | PEN | PTW | PEQ | a87 | WKS | EPR | PRS | PRT | | PRD | PRO | | | | QCC | RMP | RSR | SRM | MRM | MGR | RFR | wWm | REF | EAR | SRS | ESK | SWR | | SCU | | YFh | SIL | ESR | LrD | YnJ | ESP | MSM | Tmx | STC | OLS | k67 | JXh | PWS | TWC | EPW | TCP | TCE | WSN | TLS | MTL | STL | TGR | OTR | | | UNI | UVR | FWK | gLF | WRS | WPS | YQd

Medium Temperature Glaze Recipes

Normally fired at cone 5-7 in electric kilns.

Related Information

Links

Glossary Medium Temperature
These are stoneware glazes that fire in the range of 1200C (2200F). They often contain boron to assist with melting.
Recipes G1214W - Cone 6 Transparent Base
A cone 6 base clear glaze recipe developed by deriving a recipe from a formula taken as an average of limit formulas
Recipes G1214M - 20x5 Cone 6 Base Glossy Glaze
Developed by Tony Hansen in the 1980s. Its was popular for the simplicity and how well it worked with chrome-tin stains.
Recipes G1214Z1 - Cone 6 Silky CaO matte base glaze
This glaze was born as a demonstration of how to use chemistry to convert a glossy cone 6 glaze into a matte.
Recipes G1215U - Low Expansion Glossy Clear Cone 6
A recipe sourcing high MgO (from Ferro Frit 3249) to produce a low expansion glass resistant to crazing on lower silica porcelains.
Recipes MGBase1 - High Calcium Semimatte 1 (Mastering Glazes)
From page 86 of Mastering Glazes book
Recipes MGBase2 - High Calcium Semimatte 2 (Mastering Glazes)
Base from Mastering Glazes book page 89
Recipes MGBase3 - General Purpose Glossy Base 1 (Mastering Glazes)
From page 92 in Mastering Glazes book
Recipes MGBase4 - Glossy Base 2 Cone 6 (Mastering Glazes)
From page 96 in Mastering Glazes book
Recipes MGBase5 - Glossy Clear Liner Cone 6 (Mastering Glazes)
From page 97 of Mastering Glazes book
Recipes MGBase6 - Zinc Semimatte Glossy Base Cone 6
From page 98 of Mastering Glazes book
Recipes MGBase7 - Raspberry Cone 6 (Mastering Glazes)
From page 102 in Mastering Glazes book
Recipes MGBase8 - Waxwing Brown Cone 6 (Mastering Glazes)
From page 104 in Mastering Glazes book
Recipes MGBase9 - Waterfall Brown Cone 6 (Mastering Glazes)
From page 106 of Mastering Glazes book
Recipes GR6-A - Ravenscrag Cone 6 Clear Glossy Base
This Plainsman Cone 6 Ravenscrag Slip base is just the pure material with 20% added frit to make it melt to a glossy natural clear.
Recipes GR6-H - Ravenscrag Cone 6 Oatmeal Matte
Plainsman Cone 6 Ravenscrag Slip glaze. See more at ravenscrag.com.
Recipes g2851H - Ravenscrag Cone 6 High Calcium Matte Blue
Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.
Recipes GR6-E - Ravenscrag Cone 6 Raspberry Glossy
A chrome-tin burgundy glaze using the Ravenscrag cone 6 base recipe.
Recipes GR6-B - Ravenscrag Cone 6 Variegated Light Glossy Blue
Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.
Recipes GR6-C - Ravenscrag Cone 6 White Glossy
Plainsman Cone 6 Ravenscrag Slip based white glossy glaze. It can be found among others at http://ravenscrag.com.
Recipes GR6-D - Ravenscrag Cone 6 Glossy Black
Recipes G2928C - Ravenscrag Silky Matte for Cone 6
Plainsman Cone 6 Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy