Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Kaolinite

Formula: Al2O3.2SiO2

The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. However it makes up at least part of all ceramic clays. The purest deposits are created as it is weathered from rock and deposited, mixed with other products of the weathering process, in layers and lenses in nearby valleys. Thus kaolins (also called China Clays) are whiter and cleaner than other clays because they are mined near the site where they were weathered and altered (rather than being contaminated when transported and sedimented by water). Because kaolin ore is mixed with other rocks and impurities, it has to be separated using various wet and dry processing methods. Kaolin can be found is some sedimentary deposits where it is mixed with quartz and feldspar particles, it can be separated by wet processing methods.

Kaolinite is a pure clay mineral crystal of one part alumina and two parts silica. Most other clay minerals are derivatives of kaolin. Kaolin particles are flat and comparatively the largest of all clay minerals, this makes them among the least plastic. They have a surface chemistry that gives them an affinity for water. The attached water both 'glues' particles together and acts as a 'buffer' to lubricate particle-against-particle movement in the plastic matrix.

In it purest form, kaolin melts at 1770C, thus it is quite refractory. However this temperature drops quickly as impurities increase (like feldspar). Kaolin particles have an inner crystalline structure of alternating flat Al2O3, SiO2 and hydroxyl layers. The Al2O3 and SiO2 bind firmly but the hydroxyl layer does not. This structure accounts for the flat shape of kaolin particles and the way they stack and separate in reacting to physical forces. It also accounts for the affinity for water that the particles have and the difference in charge between the flats and edges. In addition, this structure shapes what happens as heat is applied: the hydroxyl is driven off breaking the bonds between the layers and freeing most of the SiO2 and Al2O3 react on their own. Some of the SiO2 combines to form quartz micro-crystals and some of the Al2O3 forms alumina micro-crystals. Both can dissolve in the feldspar glass. Some of the SiO2 and Al2O3 can remain connected to preserve flat kaolinite particles. Of course the way it which this all plays out is dependent on many factors, especially the firing curve.

Related Information

Links

Materials Clay 215
Materials Clay 216
Materials Clay 246
Materials Clay 220
Materials Clay 220
Materials Clay 222
Materials Clay 232
Materials Clay 233
Materials Clay 244
Materials Clay 261
Materials Feldspar 632
Materials Feldspar 635
Materials Feldspar 645
Materials Feldspar 661
Materials Kaolin 111
Materials Kaolin 113
Materials Kaolin 114
Materials Kaolin 115
Materials Kaolin 143
Materials EP Kaolin
A kaolin that gels slurries (good for suspending glazes). It has two variations: a low and medium plasticity. It fires white for use in porcelain bodies.
Materials Ryolite S1
Materials Prestige AK
Materials 3B Clay
A fine-grained, tan burning, illitic stoneware with particulate and soluble salt impurities
Materials Sterling Kaolin
Materials Topaz Kaolin
Materials Super Standard Porcelain
Materials Standard Porcelain Kaolin
Materials Sovereign Kaolin
Materials Grolleg Kaolin
A white burning kaolin from the UK, commonly used in porcelain bodies and as a glaze suspender. Sticky when wet, low plasticity.
Materials Treviscoe Kaolin
Materials NSC Kaolin
Materials Remblend Kaolin
Materials Kernick Kaolin
Materials LPC Kaolin
Materials WTD Kaolin
Materials Calcined Topaz Kaolin
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Materials Kaolin 233
URLs http://en.wikipedia.org/wiki/Kaolinite
Kaolinite on WikiPedia
URLs http://www.minersoc.org/pages/gallery/claypix/kaolinite/kaolinite_q00.html
One of a number of micrographs of kaolinite at minersoc.org
URLs http://www.handbookofmineralogy.org/pdfs/Kaolinite.pdf
Kaolinite mineralogy
Minerals Dickite
A clay mineral with the same composition as kaolinite but different crystal structure.
Minerals Allophane
A clay mineral similar to kaolinite.
Minerals Ball Clay
Ball clay is the most common type of secondary clay. They are much more plastic than kaolin because
Typecodes Clay Minerals
The property of plasticity is evident in a wide array of materials of different mineralogy. In addition, many minerals are considered parent minerals to clays, they weather down to become these clays.
Glossary Primary Clay
A clay deposit that is near the site of erosion and alteration. They have more mechanical impurities and fewer chemical and mineralogical impurities. Primary clays have larger particles and less plasticity.
Glossary Clay
What is clay? How is it different than dirt? For ceramics, the answer lies on the microscopic level with the particle shape, size and how the surfaces interact with water.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy