Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Anorthite

Formula: CaAl2Si2O8

A plagioclase feldspar (vs. typical alkali feldspars used in ceramics). More precisely, it is a calcium end-member of the plagioclase feldspar series.

Anorthite is also a crystal phase that makes bone china possible (it forms and grows during firing). Bone china is termed "anorthite porcelain" (vs typical "mullite porcelains"), more precisely it is a CaO - P2O5 - Al2O3 - SiO2 glass-ceramic system. During the firing, feldspar melts, kaolin decomposes to source free SiO2, bone ash provides CaO. The melt becomes CaO -Al2O3 - SiO2 rich. Anorthite crystallizes out of that melt. It is a recrystallization process driven by CaO reacting with an aluminosilicate melt.

Anorthite is also formed in high-calcium glazes, especially cone 9–10 lime mattes (or calcia mattes). The characteristic microcrystalline matte surfaces are typically CaO - Al2O3 - SiO2 rich. In glaze textbooks, references to “lime matte crystallization” or “calcium aluminosilicate crystals” is frequently referring to anorthite.

In Portland cement and kiln clinkers: It appears in phase diagrams and ceramic engineers studying kiln reactions encounter it frequently.

Calcium porcelains (explored historically as alternatives to feldspathic porcelain): Where CaO replaces part of the alkali flux, anorthite becomes a major crystalline phase.

In devitrification in high-CaO glazes (especially slow-cooled): Anorthite, wollastonite and other Ca silicate crystals can form.

In glaze defect analysis: Anorthite may appear in XRD results when investigating matte surfaces, devitrification, stiff calcium glazes, high calcium feldspars and calcareous clays.

Phase diagram literature: In the CaO - Al2O3 - SiO2 phase triangle (a classic in ceramic texts), anorthite is a primary phase field.

Other things get more attention in pottery literature or studio-level discussions: E.g. Mullite, quartz, cristobalite.

Related Information

Links

Minerals Plagioclase
Plagioclase feldspar is not one mineral but a series between two: Albite - NaAlSi₃O₈ (high sodium) a
Materials Calcium Feldspar
URLs http://www.handbookofmineralogy.org/pdfs/Anorthite.pdf
Anorthite mineralogy data

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy