Formula: K[AlSi2O6]
Hardness: 5.5-6 Density: 2.5
K2O 21.50%, Al2O3 23.50%, SiO2 55%
An alumino-silicate common to granites and feldspars, often accompanied by nepheline. Easily fluxed below 1000C.
| Minerals |
K-Feldspar
Most common feldspars contain both sodium and potassium. The term K-Feldspar designates one where th |
| Minerals |
Nepheline
A feldspathoid silica-undersaturated aluminosilicate mineral. |
| Materials |
Potash Feldspar
A feldspar having a KNaO content that predominates in potassium. |
| URLs |
http://en.wikipedia.org/wiki/Leucite
Leucite at Wikipedia.com |
| URLs |
http://www.handbookofmineralogy.org/pdfs/Leucite.pdf
Leucite mineralogy data |