Feldspar 661

Alternate Names: Feldspat 661

Oxide Analysis Formula Tolerance
CaO 0.52% 0.06
MgO 0.28% 0.04
K2O 8.82% 0.59
Na2O 2.96% 0.30
TiO2 0.03% -
Al2O3 16.37% 1.02
SiO2 70.69% 7.46
Fe2O3 0.10% -
LOI 0.25%n/a
Oxide Weight 633.10
Formula Weight 634.69

Notes

Available in -75, -63 and -45 micron sizes.

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Minerals Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How
Materials Feldspar 632
Materials Feldspar 645
Materials Feldspar 635
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy