Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.
Formula: Mg3B7O13Cl
Hardness: 7 Density: 2.9-3 Soluble in HCl Water insoluble
Popular flux particularly at the mid-range temperatures of 1000-1200ºC. A major boron ore and source for boric acid.

This picture has its own page with more detail, click here to see it.
Boracite Crystals
| URLs |
http://en.wikipedia.org/wiki/Boracite
Boracite on Wikipedia |
| URLs |
http://www.handbookofmineralogy.org/pdfs/Boracite.pdf
Boracite mineralogy information |
| Materials |
Boric Acid
|