Drying cracks in bricks - but no data to determine best response

Bricks cracking during drying

These bricks were being extruded in India and the plant was suffering drying cracks. A consultant recommended a high percentage addition of lignosulphonate, at a cost of $800/ton, as a solution. But before adding such a large expense, some obvious changes seemed in order first. The technician knew the plasticity index of the clay (a measurement used for soils) but he did not have records of its drying shrinkage, water permeability, drying strength or drying performance - when problems like this arise such data provides direction and help answer questions. For example, is cracking happening because of lack of drying strength or plasticity or because drying shrinkage is too high. The splitting along the corner of the extrusion is a clue that plasticity could be lacking - that could be solved by a small bentonite addition or reduction in grog. If permeability is low an increase in grog might be needed (if the pugmill can still extrude slugs with a smooth edge and corner). Notice the cracks that start from those splits (lower left). But also notice how the top edge has shrunk while the center section has not. That indicates the drying process is not tuned to subject all surfaces to equal airflow (sure enough, these are being dried outside in the sun and wind). Another factor is cross-section: The round holes create variations in thickness that exceed 300%, square holes with rounded corners would be better. Given the location, economic realities and past success this one change might be enough to make a big difference.

Context: Simple Physical Testing of.., Bricks and tiles are.., Clay lab report Is.., Physical Testing, Cracking of Clays During..

Tuesday 30th April 2024

Polar Ice slip-cast mug owes its wonkiness to Veegum

Polar ice slip cast mugs

This is possible because Polar Ice, the casting version, behaves like rubber after draining. The rims can be peeled away from the mold and the piece can be completely collapsed to forcibly peel it out of the mold. They could then be opened and dried. To add more insult to the wonky shape large pieces can be broken away at leather-hard stage and then reattached using the slip as glue - the piece will still dry normally! The 1% Veegum is solely responsible for all of this, without it the New Zealand kaolin based slip would be too fragile to even cast this.

Context: First mug in my..

Tuesday 23rd April 2024

At what point is a self-supporting cone bent to the correct degree?

A self supporting cone in an Orton guide

Orton says “90 angular degrees is considered the endpoint of cone bending”. First, let's assume the normal: Examination of cones on kiln-opening to verify controller operation. Consider the cone on the left: The tip is touching. But it is also beginning to buckle, which means it was touching for a while before the firing ended. Who knows how long! The second one is not touching but has still fallen a little too far. Why do we say that? The third one, positioned on the Orton guide, has reached the recommended 90 degrees. This demonstrates a good reason why self-supporting cones are much better than standard ones: They are not touching when considered done. And standard cones, when sent in a 3/4" plaque, have a less consistent bending behaviour.

Context: The bending of an.., Cones bending badly, Are you using your.., Manually programming a Bartlett.., What temperature do Orton.., Program your firings manually.., Cones bending theoretically cones.., Pyrometric Cone, Make Your Own Pyrometric..

Saturday 20th April 2024

This iron oxide stain on porcelain disappeared during firing?

Iron stain porcelain fires clean

This porcelain is 43% kaolin, 20% silica, 36% nepheline syenite and 1% Veegum. I cast it in a test mold that had been used for a very dark red burning body. The inner unstained section looks no different than the outside after firing to cone 6. This porcelain develops a vitreous surface, it is apparently able to dissolve and absorb the thin film of iron (unlike a stoneware). Kaolins in even very white burning porcelains always contain a small percentage of iron oxide as a contaminant, but as long as it is below about ~0.5% the fired color is not visibly darkened.

Context: This is how much..

Wednesday 17th April 2024

First mug in my newly created mold

Slip cast mug

This test mold is thin-walled yet I can cast three thick-walled mugs in three hours. This clay is L2596G, a buff burning cone 10 stoneware - the mug on the lower right has been fired to cone 10 oxidation. Achieving 4-5mm thick walls is not a problem if the casting slip employs a large particle kaolin intended for this purpose (e.g. Opticast). The flared lip works as expected, keeping the rim nice and round. No cracks have appeared at handle joins, even for pieces left in the mold overnight. The mold halves mate with each other very well and the seam is easy to remove. The seam on the base is an issue - I have to be careful to line up the halves well before clamping the mold strap - this is a warning for accuracy during the mold production stage. And the possible motive for a three-piece mold if I get more serious about this piece.

Context: AI-Imagined mug I chose.., Polar Ice slip-cast mug.., Coffee Mug Slip Casting..

Wednesday 10th April 2024

Personal size sieve shakers you can buy on Amazon

Small vibrating sieve shakers

These are small-scale devices that work on the same principles as industrial ones - thus they put industrial methods of clay processing in the hands of a potter or hobbyist. These products are stainless steel and food grade and most can be used with powders or shurries and have interchangeable screens. The most expensive device here costs $5000 and the least expensive is far less than $1000. The suppliers of each of these also have other similar machines (as well as other types of processing equipment potentially valuable in small-scale ceramic production).

Context: How to Find and.., Formulating a body using.., 11 v 22 v.., 11 v 5 w.., 22 V 5 W.., 2 8V 6 HZ.., Making your own sieve..

Sunday 24th March 2024

3D printed plaster filled case mold ready for pouring block mold

3D printed mug mold

This is part of a project to make a slip-casting mold for a coffee mug. In the slicer, I split the print into two pieces 22mm up from the base. This enabled doing the bottom section right side up and the top one upside down. That drastically cut the amount of support generated (and thus printing time). I scotch-taped the two halves together and filled it with plaster to produce a rigid block mold. The two halves fit so precisely it is difficult to tell where they join. The big benefit of printing it upright like this is that the all-important front face is very flat (there is some warpage on other parts but that does not matter).

Context: Coffee Mug Slip Casting..

Wednesday 20th March 2024

3D design, printing and use of a slip clay test bar mold

SHAB mold for casting clays

This is for making test bars of slip casting clays bodies for use in the SHAB test (to measure drying shrinkage, firing shrinkage and fired porosity). I designed it in Fusion 360 and 3D printed the light-duty rails and case mold. I poured plaster into that to make the two plaster working mold halves (top right). The funnels provide a reservoir so the bars be cast solid. This mold can produce a set of three bars in less than an hour.

Context: Shrinkage/Absorption Test, Side Rails

Tuesday 19th March 2024

Lead bisilicate with his ugly borosilicate cousins at a cone 05 party

Boron and lead transparent glazes on terra cotta

The middle front mug is glazed with an 85:15 lead bisilicate:kaolin mix, the G3971 recipe. It is an absolutely "knock your socks off" crystal-clear hyper-glossy surface that transmits the terra cotta color beautifully regardless of whether the clay is smooth or coarse or the glaze thick or thin (this one was applied as a brushing glaze in three coats on L215). My lead testing kit passes it with no detectable lead release. The other pieces are done using brush-on versions of boron-based clear glazes (commercial and made from a recipe). At almost any thickness and whether on L215 or L4170B clouding occurs. The worst one is a commercial three-coater on the right, the best is G1916W (it has 2% added iron as a fining agent for the micro-bubbles). My terra cotta plan: Glaze the inside functional surfaces with that and the outsides with the leaded one (and using a kiln exhaust system).

Context: Lead Bisilicate Frit, A lead bisilicate frit.., 2 iron oxide in.., Boron blue in low.., A cure for long-time.., Is it impossible to.., Thick application clouds a.., Lead in Ceramic Glazes..

Sunday 17th March 2024

A better cone 6 oatmeal glaze using Ravenscrag Slip

Ravenscrag oatmeal glazed mug

Left: G3933EF oatmeal based on Ravenscrag Slip.
Right: G3933 oatmeal based on a mix of G2934 matte and G2926B glossy base glazes.
Both have the same added colorants. The Ravenscrag version features several advantages. Most importantly much less tendency to crawl. It has better application properties, the slurry needs less water and it is naturally thixotropic. It has an extra option for adjusting properties: Changing the ratio of roast-to-raw Ravenscrag clay. It is responsive to cooling differences - more matte on slow cool versions of the C6DHSC schedule (e.g. 150F/hr), more glossy on faster cools (e.g. 250F/hr). And, its recipe is adjustable (e.g. raising the MgO if a more persistent matte is needed). And, it looks and feels way better, interacting with dark bodies for richer color and varying in tone more for thinner and thicker sections.

Context: Ravenscrag Slip, Sometimes it is better..

Wednesday 13th March 2024

Contact Me

Use the contact form at the bottom on almost all the pages on this site or let's have a together.

Other ways to Support My Work

Subscribe to Insight-Live.com. It is about doing testing and development, not letting the information slip away. Starts at $15 for 6 months.

Tony Hansen
Follow me on

Test, Document, Learn, Repeat in your account at insight-live.com

Login to your online account

Chemistry plus physics. Maintain your recipes, test results, firing schedules, pictures, materials, projects, etc. Access your data from any connected device. Import desktop Insight data (and of other products). Group accounts for industry and education. Private accounts for potters. Get started.

Conquer the Glaze Dragon With Digitalfire Reference info and software

Download for Mac, PC, Linux

Interactive glaze chemistry for the desktop. Free (no longer in development but still maintained, M1 Mac version now available). Download here or in the Files panel within your Insight-live.com account.


What people have said about Digitalfire

  • Your website is phenomenal, I love it to get insight on different oxides. I helps me alot, even though we are pretty specialized.
  • I'm still reading about expansion and some of what you explained to me is in this article by digital ... so much lay men terms and analogies makes its more viewable to the mind and understandable... thanks - I continue to say thanks... Tony.... :)
  • First I want to thank you for creating and maintaining your web site. I started as a potter and moved into ceramic engineering over the course of my career and your web site has helped me all the way. Currently I am working on digital ceramic ink jet printing.
  • Nice to know you are out there to lend us a hand. You are very much appreciated by this potter and many more, I am sure.
  • Honestly I do not see how you have time to experiment, test, etc. and disseminate the massive amount of knowledge you have.
  • We have been aware of your company and website for many years and see it as a model in its approach to educating makers about the processes involved in making/drying/firing. You teach them to take responsibility for their work process rather than blaming the product.
  • First, let me thank you for creating such a wonderful, informative, and comprehensive site. I know that I will spend many a long hour pouring through your pages.

What people have said about Insight-Live

  • I am a production potter and I have been using your website for information, and I have made many improvements from articles posted on this site.
  • I am a long time admirer of your ceramics data base and teach at ... University.
  • I love insight BTW. I have been showing everyone at Alfred how easy it is to do UMF while comparing two recipes next to each other. The up and down toggles make it easy to understand cause and effect. They are also impressed how easily i can switch between my computer and smartphone and maintain all my work and recipes. BTW I just love insight. It has changed my experience and knowledge of glazes drastically.
  • Your site is great! It is so good to have your site as I venture into making my food-safe glazes. I live in São Paulo, Brazil, so the raw materials here naturally can be very different from the ones in most of the books and websites, as we don't have much of that available here. So your site is the only that I have found so far that is really helpful if you want to start from scratch, so thank you! Its like my dream as a potter to make beautiful, lasting and safe ware so your website and insight-live are invaluable sources of information for me. I am so glad to be able to work with this! I really admire your work and tell my students about your website. Here in Brazil, studio ceramics is not a very developed area. Many people don not even know/care about being precise and knowledgable about safety with glazes. So your website is like an oasis in the tropical desert.
  • This is really cool. Thanks for sending this to my email.
  • THIS IS FRIGGIN' AMAZING! YAY! NOW I NEED GLAZE MATERIALS! WOOT! I'm blown away by your site. I'm totally going to geek out on this I can tell. Item #1 on my agenda is to stop being at everyone else's mercy for glazes.
  • I use the site often and appreciate all the information you share so willingly. Mostly the site is a fantastic reference and has profoundly improved my understanding of glaze chemistry.



https://digitalfire.com, All Rights Reserved
Privacy Policy

1