Introduction

The study of materials is at the center of ceramic technology. While oxide chemistry helps us understand and adjust the fired properties of glazes, it is the physical, mineralogical and chemical characteristics of actual materials that determine how they behave during forming, drying and firing. Ceramic technicians work with real-world materials, not just theoretical oxides. These materials have plasticities, particle-size distributions, surface areas, solubilities, melting behaviours, firing characteristics, impurities, costs and consistency issues. Knowing these properties is essential to formulating, testing and troubleshooting ceramic bodies and glazes.

Most ceramic materials are supplied as processed powders, although some are available as granules, liquids or prepared mixtures. Their properties depend not only on what minerals they contain, but also on how they have been mined, refined, classified, blended and processed. Two materials having similar chemical analyses, or even the same mineralogical composition, can behave quite differently in actual use. A change in particle size, for example, can dramatically affect plasticity, drying shrinkage, casting rate, glaze suspension or melting behaviour without significantly changing the chemistry.

Understanding problems at different levels

Materials must be understood in the context of the other levels of ceramic technology: oxide, mineral, material, recipe and process. Knowing which level is responsible for a problem is often the key to solving it. Consider a clay body that cracks during drying. The cause might be uneven drying, a process-level problem. Or the recipe might contain too much highly plastic ball clay, producing excessive drying shrinkage. A change in the particle-size distribution or plasticity of one of the supplied materials might also be responsible. In more difficult cases, understanding the mineralogy and particle characteristics of the ingredients may be necessary. The same visible defect can have very different causes, and the appropriate solution depends on identifying them. Sometimes a problem involves several levels at once. Consider a glaze slurry that settles rapidly, dries to a powdery surface and adheres poorly to ware. These symptoms may indicate inadequate clay content. If the fired glaze is also excessively fluid, adding kaolin could potentially address both problems. Kaolin can improve suspension and dry hardness while supplying Al2O3 and SiO2 to stiffen the fired melt. One recipe change can thus improve both working and fired properties!

Chemistry, mineralogy and materials are different

The same substance can be viewed very differently at each level. Consider kaolin. At the material level, it is a powder having measurable plasticity, drying shrinkage, particle size, casting behaviour and firing characteristics. At the mineral level, its principal constituent is kaolinite, whose crystal structure, particle shape and surface chemistry help explain these properties. At the oxide level, kaolin is primarily a source of Al2O3 and SiO2. These perspectives are complementary, not interchangeable. Two kaolins having nearly identical oxide analyses can differ substantially in plasticity, drying behaviour and casting performance. Likewise, two glaze materials supplying the same oxides may not release them into the developing melt at the same rate or temperature. Mineralogy, particle size and firing conditions can make a significant difference, even when calculated oxide chemistry is unchanged. Thus ceramic formulation cannot be reduced to chemistry alone. Understanding the materials that supply the chemistry is just as important.

Generic materials and commercial products

Digitalfire distinguishes between generic materials and specific commercial products. For example, the generic kaolin record contains information common to kaolins as a class. Individual commercial kaolins are linked to that record, with their own chemistry, physical properties, supplier information and application-specific behaviour documented separately. The generic kaolin record is, in turn, linked to the mineral kaolinite. This organization avoids duplicating information while connecting material properties to the underlying mineralogy and chemistry. It also makes it easier to compare alternatives, evaluate substitutions and understand why materials sold under the same generic name are not necessarily interchangeable.

Material data must be verified

Supplier data sheets are valuable, but they do not always provide the information needed for ceramic applications. Analyses may be incomplete, reported on different bases or revised over time. Physical specifications may describe properties that are useful to the supplier's primary market but not to potters or ceramic manufacturers. Some properties that matter most in ceramics, like drying shrinkage, plasticity, casting rate, firing shrinkage, absorption and melting behaviour, may not be reported at all. This is why testing materials for their actual intended use is so important. Comparative tests can reveal differences that are not apparent from chemical analyses or published specifications. They also establish a baseline against which future shipments, substitutions or changes in processing can be evaluated.

The Digitalfire materials database is intended to bring these perspectives together: chemistry, mineralogy, physical properties, fired behaviour, testing and practical experience. Its purpose is not simply to describe materials, but to help technicians understand how they work, why they sometimes fail and how to use them more effectively.

Links

Glossary Ceramic Material
Ceramic materials are employed in the ceramic industry to make glazes, bodies, engobes and refractories. We study them at the mineral, chemical and physical levels.
Glossary Theoretical Material
In glaze chemistry, theoretical materials are used to represent what a material would be if it was uncontaminated and perfectly crystallized
Glossary Physical Testing
In ceramics, glazes, engobes and bodies have chemistries and physics. Your formulation and quality control most likely need to focus on the physical properties.
Articles Chemistry vs. Matrix Blending to Create Glazes from Native Materials
Is it better to do trial and error line and matrix blending of materials to formulate glazes or is it better to use glaze chemistry right from the start?
Articles Particle Size Distribution of Ceramic Powders
Understanding the theory behind sieve selection, how to properly sample a powder and how to carry out a particle size distribution test can give you valuable information about a material.
Articles How to Find and Test Your Own Native Clays
Some of the key tests needed to really understand what a clay is and what it can be used for can be done with inexpensive equipment and simple procedures. These practical tests can give you a better picture than a data sheet full of numbers.
Hazards Overview of Material Safety by Gavin Stairs
Toxicology and ceramic materials is a complex subject, what materials and methods pose the greatest dangers, which are the safest?
Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.

Lab testing a clay for its physical properties


This picture has its own page with more detail, click here to see it.

It only takes a few minutes to make these. But you would be amazed at how much information they can give you about a clay! These are SHAB test bars, an LDW test for water content and a DFAC test disk about to be put into a drier. The SHAB bars shrink during drying and firing, the length is measured at each stage. The LDW sample is weighed wet, dry and fired. The tin can prevents the inner portion of the DFAC disk from drying and this sets up stresses that cause it to crack. The nature of the cracking pattern and its magnitude are recorded as a Drying Factor. The numbers from all of these measurements are recorded in my account at Insight-live. It can present a complete physical properties report that calculates things like drying shrinkage, firing shrinkage, water content and LOI (from the measured values).

Refined 200 mesh materials are not guaranteed to be such


This picture has its own page with more detail, click here to see it.

Each of these eight pallets of kaolin are being sampled to screen them for oversize particles. The 50 gram samples needed can be taken without having to open the bags, they are filled through a valve at the top and it can be opened easily. Kaolins and ball clays especially are suspect and body manufacturers must be vigilant about this (each can tell you disaster stories about making product with faulty raw materials containing grit, carbon and iron particles). The samples will be washed through 70, 100 and 150 mesh screens to spot any particles that could introduce grit or fired speckle into the bodies.

Do not rely on material data sheets, do the testing


This picture has its own page with more detail, click here to see it.

The cone 6 porcelain on the left uses Grolleg kaolin, the right uses Tile #6 kaolin. The Grolleg body needs 5-10% less feldspar to vitrify it to zero porosity. It thus contains more kaolin, yet it fires significantly whiter. Theoretically this seems simple. Tile #6 contains alot more iron than Grolleg. Wrong! According to the data sheets, Grolleg has the more iron of the two. Why does it always fire whiter? I actually do not know. But the point is, do not rely totally on numbers on data sheets, do the testing yourself.

Lignite contamination in manufactured porcelain body


This picture has its own page with more detail, click here to see it.

These contaminating particles are exposed on the rim of a bisque-fired mug. The liqnite ones have burned away but the iron particle is still there (and will produce a speck in the glaze). Remnants of the lignite remain inside the matrix and can pinhole glazes. Since ball clays are air floated (a stream of air takes away the lighter particles and the heavier ones recycle for regrinding) it seems that contamination like this would be impossible. But the equipment requires vigilance for correct operation, especially when there is pressure to maximize production. Ores in Tennessee are higher in coal than those in Kentucky. North American clay body manufacturers who confront ball clay suppliers with this contamination find that ceramic applications have become a very small part of the total ball clay market - complaints are not taken with the same seriousness as in the past.

When both mineralogy and chemistry are shown on a data sheet


This picture has its own page with more detail, click here to see it.

Some material data sheets show both the oxide and mineralogical analyses. Dolomite, for example, is composed of calcium carbonate and magnesium carbonate minerals, these can be separated mechanically. Although this material participates in the glaze melt to source the MgO and CaO (which are oxides), it's mineralogy (the calcium and magnesium carbonates) specifically accounts for the unique way it decomposes and melts.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy