Quartz 741

Alternate Names: Kuvars 741

Oxide Analysis Formula Tolerance
CaO 0.08% 0.27
MgO 0.08% 0.38
K2O 0.04% 0.08
Na2O 0.09% 0.27
TiO2 0.03% 0.07
Al2O3 0.30% 0.56
SiO2 99.20% 312.17
Fe2O3 0.04% 0.05
LOI 0.14%n/a
Oxide Weight 18,886.49
Formula Weight 18,912.97

Notes

Available in -100, -63 and -45 micron sizes.

Related Information

Links

Materials Quartz 761
Materials Quartz 762
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy