Quantum K200 Feldspar

Description: Thai Feldspar

Oxide Analysis Formula Tolerance
SiO2 66.90% 6.69
TiO2 0.02% -
Al2O3 18.14% 1.07
Fe2O3 0.16% 0.01
Na2O 2.96% 0.29
K2O 11.17% 0.71
Oxide Weight 597.34
Formula Weight 597.34