Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Plagioclase

Formula: NaAlSi3O8 to CaAl2Si2O8

Plagioclase feldspar is not one mineral but a series between two: Albite - NaAlSi₃O₈ (high sodium) and Anorthite - CaAl₂Si₂O₈ (high calcium). Thus, every plagioclase is some mixture of those two. The more sodium (Na₂O), the closer to albite; the more calcium (CaO), the closer to anorthite.

Plagioclase is a primary flux source in many clays, a natural contributor to vitrification in stoneware and the backbone of porcelain vitrification. It is also a primary flux source in many glazes. It often crystallizes as anorthite in high-calcium bodies and glazes.

Albite is lower melting, has higher thermal expansion, and stronger fluxing action. Is produces more glassy, less crystalline glasses/glazes.

Anorthite is higher melting, lower thermal expansion and promotes crystal formation (anorthite). It tends to producet ougher, more stable melts.

Most stoneware and porcelain bodies contain plagioclase as ground feldspar. Some clays also contain natural feldspar. During firing, feldspar begins to melt and form a glassy phase that dissolves quartz and reacts with kaolin. In calcium-rich systems, anorthite crystals can form, these increase strength, reduce pyroplastic deformation and help thermal shock resistance.

Orthoclase (microcline) feldspars are a different group. They melt slightly higher, have less crystallizing tendency and lower thermal expansion.

Related Information

Links

Materials M74 Feldspar
Materials Andesine
URLs http://en.wikipedia.org/wiki/Plagioclase
Plagioclase on Wikipedia
URLs http://en.wikipedia.org/wiki/Albite
Albite at Wikipedia
URLs http://www.agu.org/pubs/abs/jb/98JB02300/tmp.html
Study on melting of Albite - Institute of Geophysics and Planetary Physics
URLs http://www.handbookofmineralogy.org/pdfs/Albite.pdf
Albite mineralogy data
Minerals Anorthite
A plagioclase feldspar (vs. typical alkali feldspars used in ceramics). More precisely, it is a calc
Minerals Oligoclase
A plagioclase feldspar.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy