Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Andesine

Description: Plagioclase Feldspar

Formula: Na2O.CaO.2Al2O3.8SiO2

Oxide Analysis Formula Tolerance
CaO 6.99% 0.50
Na2O 7.72% 0.50
Al2O3 25.41% 1.00
SiO2 59.88% 4.00
Oxide Weight 401.42
Formula Weight 401.42

Notes

A plagioclase feldspar. The chemistry given is theoretical, actual materials will vary.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Minerals Plagioclase
Plagioclase feldspar is not one mineral but a series between two: Albite - NaAlSi₃O₈ (high sodium) a

Data

Hardness (Moh) 6.5
Frit Softening Point 1350C
Density (Specific Gravity) 2.70

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy