44MR | APPO | AVPS | AVSC | BDGC | BDLB | BLOI | BWIW | CCON | CDRY | CEC | CLWC | CMST | COLE | COVB | CSSS | DENS | DFAC | DFDM | DIEL | DNLP | DS | DSHR | DSRN | DSTR | DTMP | EBCT | EM20 | FRFU | FRRD | FRTG | FSHR | FSTR | GBBT | GBMF | GEBR | GLAZ | GLFL | GLHD | GLLE | GSPT | GTTM | HDMI | HEGF | HMA | HMAN | HMOH | IFP | IWCT | L10M | L1M | L20M | L2M | L30M | L5 | L5M | LDW | LOI | LQLM | MDPS | MLRG | MOIP | MOR | MOR5 | MORD | OLAD | P200 | P325 | PBPO | PCE | pHPG | pHPW | PPD | PRSM | PSHP | RC | RHEO | SADR | SAMG | SCLE | SHAB | SIEV | SLBY | SOLU | SPHC | SSAB | SVWT | TGA | THCO | TNST | TREL | TRMN | TSFL | UPSD | WABS | WOPL | WRA | WSR | XREF

TGA - TGA Test

This test measures weight changes in a material as it is heated and provides a convenient method for characterizing the decomposition process in inorganics. The test results are plotted on an x-y graph as temperature vs. weight. For example, calcium oxalate monohydrate, a standard material often used to verify TGA performance, exhibits three weight losses with temperatures in an inert atmosphere that appear to represent the loss of water, carbon monoxide and carbon dioxide via the process:

CaC2O4 . H2O --> CaC2O4 --> CaCO3 --> CaO

Absolute confirmation of conclusions can be done by analyzing the gaseous by-products as there evolve. Also, if a mass spectrometry (MS) curve is overlaid onto a TGA plot a more complete understanding of the decomposition process can be had. In the case of the above material, for example, the MS curve shows that the decomposition process is more complex than shown by the TGA alone. The second weight loss produces both CO and CO2. This can be explained based on further reaction of some of the CO initially formed into CO2 and pure C (this is confirmed by the presence of grey residue in the material after heading).

TGA Analysis graph

With overlaid mass spectrometry curve


This picture has its own page with more detail, click here to see it.

Example thermogravimetric analysis of calcium carbonate


This picture has its own page with more detail, click here to see it.

TGA/DTA curves for Copper Hydroxide


This picture has its own page with more detail, click here to see it.

TGA/DTA curves showing weight loss over the temperature range.

TGA-DTA Sample curve for Copper Carbonate


This picture has its own page with more detail, click here to see it.

Variables

VAL - Value (V)

The result of the variables need to be compiled

Related Information

Links

Typecodes Material Tests
Test conducted primarily on materials use to make bodies or glazes.
Articles Organic Matter in Clays: Detailed Overview
A detailed look at what materials contain organics, what its effects are in firing (e.g. black core), what to do to deal with the problem and how to measure the amount of organics in a clay material.
Glossary TGA Test
Thermogravimetric analysis (TGA) reveals when mass loss occurs during heating

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.