Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server may not be operational under later tommorrow. The digitalfire and insight-live servers were patched on Oct 21.
The measurement is done on the powdered material after settling (settling is accelerated in the test procedure). See ASTM C-29
Use the same procedure as the g/cc bulk density test, however multiply answer by 62.42 to get lbs/cubic foot.
| Tests |
Density, loose packed (lbs/cu fut)
|
| Tests |
Bulk Density g/cc (Packed)
|
| Tests |
Density (Specific Gravity)
Measure the density of a dried clay test bar |