Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability recently discovered. Servers were upgraded ahead of schedule on Oct 21. This could cause some issues. Please contact us if you encounter any.

44MR | APPO | AVPS | AVSC | BDGC | BDLB | BLOI | BWIW | CCON | CDRY | CEC | CLWC | CMST | COLE | COVB | CSSS | DENS | DFAC | DFDM | DIEL | DNLP | DS | DSHR | DSRN | DSTR | DTMP | EBCT | EM20 | FRFU | FRRD | FRTG | FSHR | FSTR | GBBT | GBMF | GEBR | GLAZ | GLFL | GLHD | GLLE | GSPT | GTTM | HDMI | HEGF | HMA | HMAN | HMOH | IFP | IWCT | L10M | L1M | L20M | L2M | L30M | L5 | L5M | LDW | LOI | LQLM | MDPS | MLRG | MOIP | MOR | MOR5 | MORD | OLAD | P200 | P325 | PBPO | PCE | pHPG | pHPW | PPD | PRSM | PSHP | RC | RHEO | SADR | SAMG | SCLE | SHAB | SIEV | SLBY | SOLU | SPHC | SSAB | SVWT | TGA | THCO | TNST | TREL | TRMN | TSFL | UPSD | WABS | WOPL | WRA | WSR | XREF

DSTR - Dry Strength (Square Bars) Test

Formula for derice pounds per square inch tensile strength:

(3 * F * S) / (2 * W * D * D)

Where F = Force in lbs necessary to break the bar
S = Span in inches
W = Width of bar at break in inches
D = Depth of bar at break in inches

See DSRN test notes for more information.

Fired strength tester


This picture has its own page with more detail, click here to see it.

Round or square fired bars are subject to a force that tests their tensile strength. The strength can be calculated from the force and the dimensions of the cross section where the break occurred.

Variables

FOR - Force (V)

WID - Width (V)

DEP - Depth (V)

SPAN - Span (V)

TMP - Firing Temperature (V)

VAL - Value (V)

Related Information

Links

Articles Simple Physical Testing of Clays
Learn to test your clay bodies and clay materials and record the results in an organized way, understanding the purpose of each test and how to relate its results to changes that need to be made in process, recipe and materials.
Articles Binders for Ceramic Bodies
An overview of the major types of organic and inorganic binders used in various different ceramic industries.
Tests Dry Strength (kgf/cm2)
Measure the tensile strength of a dried clay test bar
Tests Dry Strenth (Round Bars)
Tests Fired Strength Square Bars
Tests Modulus of Rupture - Fired
Typecodes Body Tests
Tests conducted on bodies made from materials, as opposed to the materials themselves.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.