2019 Jiggering-Casting Project of Medalta 66 Mug
A cereal bowl jigger mold made using 3D printing
Beer Bottle Master Mold via 3D Printing
Better porosity for Brown Sugar Savers
Build a kiln monitoring device
Celebration Project
Coffee Mug Slip Casting Mold via 3D Printing
Comparing the Melt Fluidity of 16 Frits
Cookie Cutting clay with 3D printed cutters
Evaluating a clay's suitability for use in pottery
Make a mold for 4-gallon stackable calciners
Make Your Own Pyrometric Cones
Make your own sieve shaker to process ceramic slurries
Making a high quality ceramic tile
Making a Plaster Table
Making Bricks
Making our own kiln posts using a hand extruder
Medalta Ball Pitcher Slip Casting Mold via 3D Printing
Medalta Jug Master Mold Development
Mold Natches
Mother Nature's Porcelain - Plainsman 3B
Mug Handle Casting
Nursery plant pot mold via 3D printing
Pie-Crust Mug-Making Method
Plainsman 3D, Mother Nature's Porcelain/Stoneware
Pottery Classes
Project to Document a Shimpo Jiggering Attachment
Roll, Cut, Pull, Attach Handle-making Method
Seven reasons to do DIY underglazes
Slurry Mixing and Dewatering Your Own Clay Body
Testing a New Load of EP Kaolin
Using milk as a glaze
Videos of factory workers making holloware
Yixing Teapots

Making a high quality ceramic tile

Making a professional floor tile is about the back of the tile as well as the glazed surface. It is about a clay body that will fire strong and durable. One that is fine grained on which glazes will fire without pinhole and blister defects. About a non-plastic clay that will dust-press well and dry quickly with minimal shrinkage. And about a clay that vitrifies enough to develop the needed strength, yet not shrink so much that fired warping cannot be overcome. It is about a non-slip glaze. And, again, it is about being flat, very flat. A studio potter can actually make a flat tile, that is amazing. A small scale operation should be able to automate enough to make custom tile viable.

More information coming soon.

Related Information

The back on my first tile


This picture has its own page with more detail, click here to see it.

I rolled the clay over the tile and cut it to size using a fettling knife. The clay is vitreous, but it is not fine-particled enough to produce clean edges and corners. The reason for the raised edge on commercial tiles become clear on this first firing: The glaze can go right to the bottom edge without being in danger of coming into contact with the kiln shelf. Of course, because it was not cut using a cookie cutter, the edges and corners are not nearly as straight and perfect as they should be.

3D drawing of the shell mold


This picture has its own page with more detail, click here to see it.

I pour plaster into this 3D-printed shell mold to create a working plaster test mold. Then I press and roll the clay into that plaster form. Then I lay stretch plastic wrap over the rolled surface. The subsequent cut (using the printed cookie cutter shown) rounds the edges perfectly as the plastic stretches downward into the cut.

It possible to make a thin flat porcelain tile from a plastic pottery body


A thin flat porcelain tile

This picture has its own page with more detail, click here to see it.

Yes. The body is Plainsman M370 (~ 25 silica, 25 feldspar, 30 kaolin, 20 ball clay + talc to tune maturity), a plastic throwing clay with far too much drying shrinkage to be suitable for tile. It is 3.8 mm thick fired (vs. commercial tiles are 5-7mm) and 33cm (13 in) square. It dried absolutely flat between sheets of plasterboard. We have even achieved total flat drying at this size using Polar Ice. Bisque and glaze firing were on an alumina shelf in an electric pottery kiln (at 300F/hr up through quartz inversion on the glaze firing), a completely unsuitable method for firing tile evenly top and bottom. Cooling on both firings was free-fall in a fairly empty kiln. Yet, it is flat! And flexible enough that I could lay it on the cement floor and stand on it without it breaking! Of course, to produce these consistently, special furniture that sinks minimal heat and a kiln that can evenly apply it front and back are needed. This is doable for custom applications. Of course, to compete in the commercial market, they need to be dust-pressed and there are lots of specifications to meet.

Links

Projects Plainsman 3D, Mother Nature's Porcelain/Stoneware

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy