Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Nepheline

Formula: Na3KAl4Si4O16

A feldspathoid silica-undersaturated aluminosilicate mineral.

Related Information

Links

Minerals Leucite
Hardness: 5.5-6 Density: 2.5 K2O 21.50%, Al2O3 23.50%, SiO2 55% An alumino-silicate common to gr
Materials Nepheline Syenite
URLs http://en.wikipedia.org/wiki/Nepheline
Nepheline at Wikipedia
URLs http://www.handbookofmineralogy.org/pdfs/Nepheline.pdf
Nepheline mineralogy

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy