Formula: PbCO3
Principal mineral source of lead.
| URLs |
http://en.wikipedia.org/wiki/Cerussite
Cerussite at Wikipedia |
| URLs |
http://www.handbookofmineralogy.org/pdfs/Cerussite.pdf
Cerussite mineral data |
| Materials |
Lead Carbonate
|
| Materials |
Litharge
|