Formula: SiO2
A cryptocrystalline form of silica.
| URLs |
http://en.wikipedia.org/wiki/Chalcedony
Chalcedony on Wikipedia |
| Materials |
Silica
Silica, sold as a white powder, is pure quartz mineral. Quartz is pure SiO2 silicon dioxide. It is the most abundant mineral on earth and most used in ceramics. |