Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Witherite

Formula: CaCO3

Barium carbonate mineral.

Related Information

Links

URLs http://en.wikipedia.org/wiki/Witherite
Witherite at Wikipedia
URLs http://www.handbookofmineralogy.org/pdfs/Witherite.pdf
Witherite mineralogy
Materials Barium Carbonate
A pure source of BaO for ceramic glazes. This is 77% BaO and has an LOI of 23% (lost at CO2 on firing).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy