Substance |
VEMP |
Notes |
|
Cristobalite |
0.05 mg/m3 |
Pr |
|
Quartz |
0.10 mg/m3 |
Pr, C2, EM |
|
Tridymite |
0.05 mg/m3 |
Pr |
|
Tripoli |
0.10 mg/m3 |
Pr |
By Edouard Bastarache
| Typecodes |
Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French. |
| Materials |
Silica
Silica, sold as a white powder, is pure quartz mineral. Quartz is pure SiO2 silicon dioxide. It is the most abundant mineral on earth and most used in ceramics. |
| Hazards |
Plant Ash Toxicity
The hazards of using plant and wood ash in ceramic glazes |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk