Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Hafnium Oxide Toxicty

Identification

Synonym: Hafnium Dioxide
Formula: HfO2
CAS # 12055-23-1

Source

Hafnium (Hf) is found in association with zirconium ores, production based on zircon (ZrSiO4) concentrates which contain 0.5% to 2% hafnium. This metal has outstanding corrosion resistance accounting for some of its major applications.

Compounds used in Ceramics

Toxicology of Hafnium Oxide

Routes of Entry

Inhalation, skin, and ingestion.

Effects of Overexposure

May cause pulmonary irritation. Coughing or sneezing may occur.

May cause irritation, inflammation may occur.

Ingestion may cause some discomfort. Hafnium is considered relatively non-toxic due to poor absorption of it in the alimentary tract of mammals.

Chronic Exposure

It may cause liver damage. It may also cause a benign pneumoconiosis by dust accumulation, without fibrosis and ventilatory effect, and without special predisposition to tuberculosis and/or lung cancer as encountered in silicosis and abestosis.

Medical Conditions Generally Aggravated by Exposure

Previous respiratory and eye disorders.

Carcinogenicity

Hafnium oxide is not considered a carcinogen by official regulatory bodies.

Quebec039;s Exposure Limits

VEMP : 0.5 mg/m³

References

  1. Occupational Medicine,Carl Zenz, last edition.
  2. Clinical Environmental Health and Toxic Exposures, Sullivan & Krieger; last edition.
  3. Sax039;s Dangerous Properties of Industrial Materials, Lewis C., last edition.
  4. Toxicologie Industrielle et Intoxications Professionnelles, Lauwerys R.R. last edition.
  5. Chemical Hazards of the Workplace, Proctor & Hughes, 4th edition

By Edouard Bastarache

Related Information

Links

Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy