Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

Alumina Toxicology | Ammonia and Latex Toxicity | Antimony Oxide | Are colored porcelains hazardous? | Arsenic Oxide | Asbestos Toxicity | Ball Clay | BARIUM and COMPOUNDS Toxicology | Barium Carbonate in Clay Bodies | Barium Carbonate in Glazes | Bentonite Toxicity | Beryllium Monoxide Toxicology | Bismuth Trioxide Toxicology | Boron Compounds and Their Toxicity | Brown Stain | Cadmium Toxicity | Calcium Carbonate Toxicology | Carbon Monoxide Toxicity | Cesium Toxicology | Chromium Compounds Toxicology | Clay Toxicity | Cobalt Oxide and Carbonate | Cobalt Toxicology | Copper Compounds Toxicology | Copper Oxide and Carbonate | Cristobalite Toxicity | Cryolite and Ceramics | Dealing With Dust in Ceramics | Diatomaceous Earth Toxicology | Dioxins in Clays | Epsom Salts | Eye Injuries Due to Radiation | Feldspar | Fighting Micro-Organisms in Ceramics | Fluorine Gas | Fumes from gas kilns | Gallium Oxide Toxicology | Hafnium Oxide Toxicty | Hydrofluoric Acid Toxicity | Iron oxide and Hematite | Lead Chromate | Lead in Ceramic Glazes | Lead Toxicology | Lithium Carbonate Toxicity | Lithium Toxicology | Man-Made Vitreous Fibers (MMVF) Toxicology | Man-Made Vitreous Fibers Safety Update | Manganese and Parkinsons by Jane Watkins | Manganese in Clay Bodies | Manganese Inorganic Compounds Toxicology | Manganese Toxicity by Elke Blodgett | Manganese: Creativity and Illness by Dierdre O'Reilly | Molybdenum Compounds Toxicology | Nickel Compounds Toxicity | Niobium Oxide Toxicity | Occupational Dermatoses | Overview of Material Safety by Gavin Stairs | Paraffin Toxicology | Perlite Toxicity | Plant Ash Toxicity | Potassium Carbonate Toxicity | Pregnancy and Ceramics | Propane Toxicology | Quartz Toxicity | Quartz Toxicity on Clayart | Rare Earth Compounds Toxicity | Rubidium and Cesium Toxicology | Rutile Toxicology | Silicosis and Screening | Silver Compounds Toxicology | Sodium Azide Toxicology | Sodium Carbonate Toxicology | Sodium Silicate Powder Toxicology | Stannous Chloride Toxicity | Strontium Carbonate Toxicity Note | Sulfur Dioxide Toxicity | Talc Hazards Overview | Talc Toxicology | Thallium Oxide Toxicology | Thorium Dioxide Toxicity | Tin Inorganic Compounds | Titanium Dioxide Toxicology | Toxicological Assessment of Zeolites | Tungsten Compounds Toxicology | Understanding Acronyms on MSDS's | Uranium and Ceramics | Vanadium and Compounds Toxicology | Vermiculite | Zinc Compounds Toxicology | Zirconium Compounds Toxicity | Zirconium Encapsulated Stains Toxicity

Calcium Carbonate Toxicology

Identification and Uses

CAS Number: 471-34-1

Molecular formula: CaCO₃

Uses and Emission Sources

Toxicology

This product is absorbed by the respiratory tract.

I - Acute Exposure

A - Inhalation

Excessive concentrations of this nuisance dust may cause coughing, sneezing, and irritation of the nasal mucosal membranes.

B - Ingestion

Not toxic.

C - Skin Contact

Skin overexposure does not represent a health hazard.

D - Ocular Contact

There is no information available but dusts could cause mechanical irritation.

II - Chronic Exposure

Excessive doses by ingestion may cause alkalosis and hyperkalemia.

Effects on Development

No data concerning any antenatal developmental effect has been found in the consulted documentary sources.

Carcinogenic Effects

No data concerning any carcinogenic effect has been found in the consulted documentary sources.

Mutagenic Effects

No data concerning any mutagenic in vivo or in vitro effect on cells of mammals has been found in the consulted documentary sources.

First Aid

I - Inhalation

Move the worker to fresh air. Seek medical care if the individual presents respiratory problems.

II - Ingestion

If large amounts are ingested, give water to drink and seek medical advice.

III - Skin Contact

Copiously wash the affected area with water. Ask for medical advice if irritation develops.

IV - Ocular Contact

Copiously wash with running water. Ask for medical advice if irritation develops.

Québec039;s Exposure Limit

VEMP = 10 mg/m³, as total dust containing less than 1% crystalline silica.

References:


By Edouard Bastarache

Related Information

Links

Typecodes Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French.
Materials Calcium Carbonate
In ceramics, calcium carbonate is primarily a source of CaO in raw stoneware and porcelain glazes.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy