A quick way of deciding if a clay is coarser or finer than another. The is the micron size when 50% of the clay is finer and 50% is coarser.
| Tests |
Average Particle Size (Microns)
|
| Tests |
% < 10 microns
|
| Glossary |
Ultimate Particles
Utlimate particles of ceramic materials are finer than can be measured even on a 325 mesh screen. These particles are the key players in the physical presence of the material. |
| Typecodes |
Particle Tests
Tests conducted to determine particle populations, sizes, shapes, densities, surface areas, etc. |