Low toxicity by ingestion. When heated to decomposition it emits toxic vapors of niobium.
Niobium
Some niobium is found in all parts of the body.
No reports of human intoxication.
An eye and severe skin irritant.
Can cause kidney damage.
Experimentally, there is moderate fibrogenic effect on the lungs after intra-tracheal administration.
Flammable in the form of dust when exposed to flame or by chemical reaction. It ignites in fluorine, chlorine.
Sax039;s Dangerous Properties of Industrial Materials.
By Edouard Bastarache
| Typecodes |
Article by Edouard Bastarache
Edouard Bastarache is a well known doctor that has written many articles on the subject of toxicity of ceramic materials and books on technical aspects of ceramics. He writes in both English and French. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk