Petalite

Formula: LiAlSi4O10 or Li2O.Al2O3.8SiO2

Oxide Analysis Formula Tolerance
Li2O 4.87% 1.00
Al2O3 16.65% 1.00
SiO2 78.49% 8.00
Oxide Weight 612.54
Formula Weight 612.54

Notes

Petalite is a lithium aluminum silicate mineral (more simply a lithium feldspar) that is commonly used in clay bodies. It is valuable because it provides an insoluble source of lithium and has the highest Li2O:Al2O3 ratio of any natural mineral. Lithium is a strong alkaline flux and is effective over all temperature ranges. It imparts lower expansion and gives a unique color response to copper and cobalt in glazes. Some commercial versions have a chemistry that fairly closely matches the theoretical chemistry given here.

Petalite is most prized for its mineralogical properties. It is especially valuable in imparting thermal shock resistance to clay bodies because it has almost zero expansion when heated above 700C. Bodies with 60%+ petalite can take a direct flame and rapid water cooling without failure. To make a plastic clay body mix petalite with as much ball clay as needed. For a casting body, use as much kaolin as needed to achieve the desired casting properties. Bentonite can be added to either type of body to increase the petalite proportion.

One serious problem with low expansion petalite bodies is that it is very difficult to achieve glaze fit. All common glazes will craze. This is compounded at lower temperatures where the limited low-expansion silica and alumina necessary for melting raises glaze expansion. For some low-expansion bodies, it is almost impossible to match a glaze

Petalite can be used to create low expansion glazes. It is suitable for white and transparents as well because of the low iron content. It does not present the frothing problems sometimes associated with spodumene and helps improve brightness. One formula suggested by Val Cushing is petalite 76.9, talc 14.2, whiting 3.4, kaolin 5.5. This glaze is claimed to have an expansion of 0.8 x 10 -6 and fires cone 9 to 12 with a silky surface.

Spodumene and lepidolite also provide insoluble sources of lithium. However, spodumene is more refractory, thus producing more porous fired results. If a body's range needs to be extended, spodumene can thus be added in preference to silica. Petalite is slightly more refractory than lepidolite.

P.C.E.: 15
P.C.E. 45% petalite:55% F4 Feldspar: 4
P.C.E. 45% petalite:55% Nepheline Syenite: 2

A petalite clay body can be made by combining petalite and ball clay or kaolin in proportions that provide a good compromise between high petalite content and necessary plasticity.

Petalite promotes the conversion of the quartz form of silica to the cristobalite form. This has implications on the thermal expansion of the fired matrix.

Spodumene is generally a better source of Li2O for frits than petalite.

Related Information

Why Petalite and Spodumene will seldom substitute for Lithium Carbonate


Lithium carbonate vs petalite vs spodumene

This picture has its own page with more detail, click here to see it.

Of course, if a recipe only calls for 1-2% lithium carbonate, either of these might be candidates to supply the Li2O. But Petalite is 8x less concentrated and Spodumene 5x less. Not surprisingly, prices reflect this (unless availability is the issue). But when a recipe calls for 5% lithium carbonate, there is another problem: Petalite is extremely high in SiO2 and spodumene is very high in Al2O3. Introducing enough of either of them to supply the same amount of Li2O as 5% lithium carbonate can easily oversupply either. While extra SiO2 can often be accommodated because most glazes contain significant silica, bringing in a lot of Al2O3 necesitates cutting the most important normal source: Clay. The result is a slurry that does not harden and does not stay suspended.

Petalite for Lithium Carbonate:

It takes eight times as much!


This picture has its own page with more detail, click here to see it.

Here are the three common lithia source materials in a side-by-side calculation to compare their potencies. I have adjusted the material weights so that all are delivering the same amount of Li2O (assuming a recipe calling for 5% lithium carbonate).

By weight it takes 42 parts of petalite to deliver the same amount of Li2O as 5 parts lithium carbonate! But notice how much SiO2 and Al2O3 come along, major surgery on the host recipe is needed to compensate for this (if even possible). Spodumene is complicated too, it brings along so much Al2O3. That’s a problem because the most frequent existing Al2O3 supplier, clay, may have to be greatly reduced or even eliminated (producing a recipe that does not suspend in water). The other baggage both materials bring is lots of SiO2, especially petalite. Thus, replacing lithium carbonate with petalite or spodumene is not really a material substitution—it is a glaze reformulation.

Links

URLs http://en.wikipedia.org/wiki/Petalite
Petalite at Wikipedia
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Amblygonite
Materials Lepidolite
Materials Triphylite
Typecodes Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Typecodes Materials used in Denmark
Hazards Fluorine Gas
Can you be exposed to fluorine gas in ceramics. Yes, if you are using materials that contain fluorine. These are not many, but worth knowing about.
Oxides Li2O - Lithium Oxide, Lithia
Glossary Cristobalite Inversion
In ceramics, cristobalite is a form (polymorph) of silica. During firing quartz particles in porcelain can convert to cristobalite. This has implications on the thermal expansion of the fired matrix.

Data

Co-efficient of Linear Expansion 0.15
Frit Softening Point 1350C M
Density (Specific Gravity) 2.45

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy