Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

BeO (Beryllium Oxide)

Data

Frit Softening Point 2650C

Notes

-Like CaO and MgO, beryllium oxide has the amazing property of being a refractory by itself and a flux in combination with other oxides (its melting point alone is likely higher than 2500C!).

-The affect of the oxide on glaze or body chemistry is not well documented (although the uses of the actual material powder in applications like thermal conductivity, dielectric strength, corrosion and whetting resistance again molten metals, neutron absorption and metalization are well understood).

Links

Materials Beryllium Oxide
Minerals Beryl
A beryllium mineral.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy