Digitalfire will shut down on June 26. I no longer have the authority to grant exemption to a section in the Terms and Conditions of using material in the Insight-Live account from which I built the source material. While there are ways to comply with the take-down order, they are beyond my means because of how complex and large the site has become in the past 35+ years. It has been a wild ride for a shy prairie boy, thanks to everyone for your support. Insight-live.com is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Carbondale Clay

Alternate Names: Carbondale Red Clay, C-Red

Description: Deep-red-burning medium-fire clay

Oxide Analysis Formula Tolerance
CaO 0.30% 0.02
K2O 0.38% 0.02
MgO 0.26% 0.03
Na2O 0.06% -
TiO2 1.03% 0.05
Al2O3 24.30% 1.00
SiO2 49.30% 3.44
Fe2O3 12.70% 0.33
LOI 11.80%n/a
Oxide Weight 370.77
Formula Weight 420.37

Notes

No longer available, replaced by C-Red, then Guage Red. The manufacturer said: "C-Red is a fine-grained, iron-bearing, plastic clay. Great for throwing bodies or where warm color and plasticity are desired. Air floated."

Carbondale Red provided formulators with an economical source of iron oxide. Its very high iron content and refractory nature made it well suited for ceramic applications requiring bright red color. It fired to a toasty red up to about cone 3 and then turned dark red to brown (partly due to soluble salts on the surface that darken the color). This material had plasticity similar to a typical pottery clay body.

Some have suggested this as a substitute for Newman Red, however, this is much more vitreous and higher in iron.

Industrial Minerals states: "Due to the variations of naturally occurring clays and minerals which limit our quality control and the variety of applications for our products over which we have no control, our products are sold with the understanding that the user is solely responsible for determining suitability for any purpose." They were buying this material from another company and there was limited supply.

Related Information

Carbondale Red fired clay bars


This picture has its own page with more detail, click here to see it.

Top to bottom cone 5, 4, 7, 8 oxidation. This material is extremely high in iron and very red-burning.

Links

Materials Newman Red Clay
Materials Redart
The most common commercially 200 mesh available raw terra cotta clay in North America. It fires red, has low plasticity and matures a low kiln temperatures.
Materials C-Red Clay
Materials Gauge Red
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://www.clayimco.com/industrial-clays
IMCO information on their mined clays

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy