Alternate Names: Guage Red, Gage Red

Description: High iron fireclay

Oxide Analysis Formula Tolerance
SiO2 40.80% 2.47
Al2O3 28.00% 1.00
Fe2O3 18.10% 0.41
TiO2 1.20% 0.05
MgO 0.20% 0.02
K2O 0.14% 0.01
LOI 10.00%n/a
Oxide Weight 326.55
Formula Weight 362.83

Notes

Replaced Carbondale Red and C-Red in 2021.

~5% retained on 200 mesh screen.
~8% quartz mineral.
Cone 04 water absorption: 23%
Cone 5 water absorption: 16%
Cone 10 water absorption: 11%
Cone 10R water absorption: 2%

In 2024 this is only being sold to selected customers, only about 800 tons per year are being mined.

Related Information

Links

Materials Carbondale Clay
A deep red burning plastic clay with 13% Fe2O3.
Materials C-Red Clay
URLs https://www.clayimco.com/industrial-clays
IMCO information on their mined clays

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy