Body Color | Body Maturity | Body Plasticity | Body Thermal Expansion | Crystal Glaze Variations | Deflocculant | | Glaze Crystallization | Glaze Matteness | Glaze Opacifier | Glaze Surface Texture | Glaze Suspender | Glaze Variegation

Glaze Color Property

Glaze color is a combination of chemistry between the colorant and host, firing process and the amount and nature of the colorant. It is possible to achieve very similar colors using very different systems, and very different colors by making very small changes in a system. Often the trade offs associated with different approaches to making a similar color can be quite complex.

Mechanisms

Recipes GC106-GC106 Base Crystalline Glaze
Materials Stain (green)
Oxides MnO2
Materials Stain (blacks)
Oxides Cr2O3
Oxides FeO
Materials Rutile
Oxides Li2O
Oxides K2O
Oxides CuO
Oxides Fe2O3
Oxides FeO
Oxides NiO
Oxides CoO
Oxides B2O3
Oxides CoO
Oxides CoO
Oxides CoO
Oxides Cu2O
Oxides CoO
Oxides CoO
Materials Manganese Carbonate
Materials Stain (blue/green)
Materials Fusion Frit FL-31
Materials Fusion Frit FL-31
Materials Fusion Frit FL-31
Oxides MnO
Materials Rutile
Oxides Cr2O3
Oxides Fe2O3
Oxides FeO
Oxides MnO
Oxides NiO
Oxides FeO
Oxides K2O
Oxides Al2O3
Oxides Na2O
Oxides K2O
Oxides K2O
Oxides Na2O
Materials Ferro Frit 3230
Materials Stain 6031
Oxides ZrO
Oxides CaO
Recipes GRNTCG-GRANITE Crystalline Glaze
Oxides Cr2O3
Materials Rutile
Oxides CuO
Oxides NiO
Oxides Cr2O3
Oxides CuO
Materials Stain (green/blue-green)
Oxides NiO
Materials Stain (grey)
Oxides CoO
Materials Ferro Frit 3230
Materials Manganese Dioxide
Oxides Cu2O
Oxides CuO
Recipes FAAO-Fa's All-Opaque Crystalline Glaze
Recipes BORY1-Bory 1 Crystalline Glaze
Materials Stain (orange)
Materials Rutile
Recipes CELECG-Celestite Crystalline Glaze
Oxides Al2O3
Oxides Li2O
Oxides NiO
Oxides SnO2
Materials Stain (pinks)
Materials Stain 6023
Oxides K2O
Oxides Cr2O3
Oxides CoO
Materials Manganese Carbonate
Oxides Cu2O
Oxides Cr2O3
Materials Stain (purple, lilac, violet)
Oxides MnO2
Oxides Se
Oxides CdO
Oxides TiO2
Oxides U3O8
Materials Silicon Carbide
Oxides CoO
Oxides Cu2O
Oxides Cr2O3
Oxides ZnO
Materials Stain (brown)
Oxides Fe2O3
Oxides FeO
Oxides NiO
Materials Rutile
Oxides K2O
Oxides BaO
Oxides Cu2O
Oxides CuO
Recipes TNF2CG-Tin Foil II Crystalline Glaze
Oxides K2O
Oxides CdO

Links

Materials Stain
Glossary Colorant
In ceramics and pottery, colorants are added to glazes as metal oxides, metal-oxide-containing raw materials or as manufactured stains.
Glossary Transparent Glazes
Every glossy ceramic glaze is actually a base transparent with added opacifiers and colorants. So understand how to make a good transparent, then build other glazes on it.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.