Description: Greens (CrCa)
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Stain
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Oxides | Cr2O3 - Chrome Oxide |
| Glaze Color | Remove any zinc from the host glaze formula, because it turns chromium brown in most situations. Additional calcium may help. |
|---|