Stain (brown)

Description: Brown Stains (FeCrZnAl, FeCr, FeCrZn)

Notes

The darkest shades of ceramic browns are based on calcined mixtures of iron and chrome oxides (with possible additions of manganese and nickel). Successively lighter shades are produced by the addition of zinc oxide and alumina.

Color Range
-----------
Black through dark brown, red brown and light brown to yellow brown and fawn.

Specific Gravity: 4.5-4.75
----------------

Stability/Kiln Atmosphere
-------------------------
Stable at temperatures up to 1300C under both oxidizing and slightly reducing conditions. Some tendency to flash or strike owing to volatility of the chrome.

Dark, zinc-free stains should be used in zinc-free glazes. The presence of zinc lightens and reddens the shade, zinc-containing stains should be used in zinc-containing glazes; red shades or red-browns are developed by glazes containing about 5% zinc oxide.

Compatibility
-------------
Suitable for blending with all types of ceramic colors except chrome-tin pinks. The zinc-free iron-chrome based browns are, however, suitable for blending with chrome-tin pinks.

Cost
----
Relatively low.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Mechanisms

Glaze ColorThe host glaze should contain from 3-5% zinc to support the red side of the stain (to get a red-brown color).

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy