Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Please don't panic, I am overwhelmed by the unbelievable support I am getting. We just need to get them to relent on this demand and call off the lawyer (to at least permit commentary). There are lots of backup sites (many people have the API endpoints), don't start downloading or scraping again and overload the server.

Insight-live.com general operation is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit VO 6200

Description: Reimbold & Strick fast firing opaque frit

Oxide Analysis Formula Tolerance
CaO 8.00% 0.36
Na2O 1.00% 0.04
B2O3 6.00% 0.22
ZrO2 9.00% 0.18
K2O 4.00% 0.11
MgO 2.00% 0.12
SiO2 53.00% 2.21
ZnO 12.00% 0.37
Al2O3 5.00% 0.12
Oxide Weight 251.10
Formula Weight 251.10

Related Information

Polar Ice Porcelain with Body Stains - by Robert Barritz


Buttons of fired porcelain of many colors

This picture has its own page with more detail, click here to see it.

Robert has done really valuable work in this research, what an amazing range of color! Surfaces are unpolished and unglazed. All are fired to cone 6. Browns are missing, they can be made using iron oxide. For blacks, Mason 6600 is also effective. The blues can be intense using lower percentages than shown here, as low as 2% can be effective. There is an optimal amount for each stain, beyond that, increases in percentage bring little increase in color intensity. There is another reason to keep stain percentages to a minimum: To reduce the impact on body maturity (and firing shrinkage). Blues, for example, can significantly heighten the degree of vitrification, even melting the porcelain. If you plan to marble different colors, keeping stain percentage as low as possible is even more important, unless you can do fired shrinkage compatibility testing, for example, the EBCT test. Need to develop your own white porcelain? See the link below.

Stains in bodies will usually bleed color into glazes used over them, especially if the body is vitreous. This can be leveraged to create or amplify variegation. Strangely, stains can increase micro bubbles in transparent glazes.

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
Frit Softening Point 790C
Glass Transition Temperature 620C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy