Alternate Names: AP Green, A.P., A. P., APG Fire, APGFC
Description: Buff Burning Plastic Fireclay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.35% | 0.02 | |
| K2O | 0.50% | 0.02 | |
| MgO | 0.35% | 0.03 | |
| Na2O | 0.50% | 0.03 | |
| TiO2 | 2.00% | 0.08 | |
| Al2O3 | 31.00% | 1.00 | |
| SiO2 | 52.00% | 2.85 | |
| Fe2O3 | 2.00% | 0.04 | |
| LOI | 11.00% | n/a | |
| Oxide Weight | 291.85 | ||
| Formula Weight | 327.92 | ||
A popular medium plasticity buff burning clay used in stoneware, sculpture and many other types of clay bodies. It is very refractory (8-10% absorption, 12% total shrinkage cone 10) and fires to an attractive surface. It is considered very consistent.
It is also used for mortar for building kilns.
20 mesh grade:
0-0.5% on 14 mesh
0.5-10.0 on 20 mesh
35.0-50.0 through 100 mesh
28 mesh grade:
0.5-5.0 on 20 mesh
0.5-10.0 on 28 mesh
20.0-38.0 through 100 mesh
PCE; 30-31.5
| Articles |
Duplicating AP Green Fireclay
Few people actually understood what AP Green fireclay really was (it is no longer available). By carefully ascertaining its physical properties we were able to formulate a substitute material mix. |
| Materials |
NAT Dry Milled Fireclay
|
| Materials |
Hawthorn Bond
|
| Materials |
Pine Lake Fireclay
|
| Materials |
Plainsman Fireclay
|
| Materials |
Imco 400 Fireclay
|
| Materials |
Fireclay
|
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Typecodes |
Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more. |
| URLs |
https://www.asbestos.com/companies/a-p-green-industries.php
AP Green Asbestos Use |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk