Description: Low temperature red earthware, terra cotta
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.81% | 0.12 | |
| K2O | 3.60% | 0.31 | |
| MgO | 1.88% | 0.38 | |
| Na2O | 1.40% | 0.18 | |
| TiO2 | 0.59% | 0.06 | |
| Al2O3 | 14.50% | 1.16 | |
| P2O5 | 0.15% | 0.01 | |
| SiO2 | 64.40% | 8.72 | |
| Fe2O3 | 5.18% | 0.26 | |
| MnO | 0.07% | 0.01 | |
| LOI | 6.50% | n/a | |
| Oxide Weight | 753.01 | ||
| Formula Weight | 805.36 | ||
A very plastic low temperature red burning terra cotta clay that was mined, by I-XL Industries, near Elkwater, Alberta, Canada. It was originally described as a clay "consisting largely of illite and free silica with a bit of free siderite as small concretions or crystals between the grains". That being said, in physical terms it was a low-temperature terra cotta clay, vitrifying by cone 1 because of the presence of significant feldspar. It was fairly high in soluble salts and required barium carbonate to precipitate these in production bodies. Hundreds of thousands of tons were used to make brick and vitrified pipe. Plainsman Clays also used this for many years to make terra cotta clay bodies and as a source of feldspar in middle-temperature red and brown stonewares. No longer available.
In later years BGP and 98 Mix were used for similar purposes.

This picture has its own page with more detail, click here to see it.
Fired from cone 5 (top) down to cone 1 (bottom).
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Materials |
IXL 45D
|
| Materials |