Alternate Names: Minium, Lead(II,IV) oxide, lead tetroxide
Formula: Pb₃O₄
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 97.67% | 1.00 | |
| LOI | 2.33% | n/a | |
| Oxide Weight | 223.20 | ||
| Formula Weight | 228.52 | ||
Red lead is a heavy, bright orange-red chemical compound. A potent low-fire flux and metal oxide color enhancer. Once popular for its ability to produce glazes of very good flow qualities, without pinholes or other defects. It also has powerful and vibrant color responses to metallic oxides.
Red lead is highly toxic if absorbed, inhaled, or ingested. Due to severe health and environmental toxicity concerns, it has largely been replaced by lead bisilicate frits.
| Hazards |
Lead Toxicology
|
| Hazards |
Lead in Ceramic Glazes
Lead glazes may or may not be hazardous. This topic is not as clear as you might think. |
| Typecodes |
Generic Material
Generic materials are those with no brand name. Normally they are theoretical, the chemistry portrays what a specimen would be if it had no contamination. Generic materials are helpful in educational situations where students need to study material theory (later they graduate to dealing with real world materials). They are also helpful where the chemistry of an actual material is not known. Often the accuracy of calculations is sufficient using generic materials. |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| Oxides | PbO - Lead Oxide |
| Materials |
Litharge
|
| Materials |
Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable. |
| Frit Softening Point | 880C M |
|---|---|
| Density (Specific Gravity) | 9.00 |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |