Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Step | °C | °F | Hold | Time | |
|---|---|---|---|---|---|
| 2 | 66°C/hr to 121C | 120°F/hr to 250F | 1:27 | ||
| 3 | 222°C/hr to 913C | 400°F/hr to 1676F | 5:01 | ||
| 4 | 66°C/hr to 1052C | 120°F/hr to 1926F | 7:06 |

This picture has its own page with more detail, click here to see it.
I document programs in my account at insight-live.com, then print them out and enter them into the controller. This controller can hold six, it calls them Users. The one I last edited is the one that runs when I press "Start". When I press the "Enter Program" button it asks which User: I key in "2" (for my cone 6 lab tests). It asks how many segments: I press Enter to accept the 3 (remember, I am editing the program). After that it asks questions about each step (rows 2, 3, 4): the Ramp "rA" (degrees F/hr), the Temperature to go to (°F) to and the Hold time in minutes (HLdx). In this program I am heating at 300F/hr to 240F and holding 60 minutes, then 400/hr to 2095 and holding zero minutes, then at 108/hr to 2195 and holding 10 minutes. The last step is to set a temperature where an alarm should start sounding (I set 9999 so it will never sound). When complete it reads "Idle". Then I press the "Start" button to begin. If I want to change it I press the "Stop" button. Those ten other buttons? Don't use them, automatic firing is not accurate. One more thing: If it is not responding to "Enter Program" press the Stop button first.
| Firing Schedules |
Bartlett Fast Glaze Cone 05
Two steps, 570F/hr to 250F below end then 200F/hr to finish |
| Firing Schedules |
Plainsman Electric Bisque Firing Schedule
Three-step to 1832F |
| URLs |
https://www.greatkilns.com/media/pdf/operating-manuals/V6CF_Manual.pdf
Bartlett V6-CF hobby kiln controller instruction manual |