Body Color | Body Maturity | Body Plasticity | Body Thermal Expansion | Crystal Glaze Variations | Deflocculant | Glaze Color | Glaze Crystallization | Glaze Matteness | Glaze Opacifier | Glaze Surface Texture | Glaze Suspender | Glaze Variegation

Glaze Variegation Property

In contrast to the typical homogeneous surfaces of sanitaryware and most table ware, reactive glazes exhibit discontinuities in texture, matteness, reflectivity, color, etc that are called variegation. These variations are normally caused by crystallization, speckling and rivulets and opacity variations associated with phase separation. By understanding these mechanisms it is possible to produce glazes of more interesting appearance.

Mechanisms

Oxides ZrO
Oxides Li2O
Oxides CaO
Materials Iron Oxide Red
Oxides P2O5
Materials Ilmenite
Materials Rutile
Materials Granular Ilmenite
Materials Granular Rutile
Materials Tin Oxide
Materials Titanium Dioxide
Oxides TiO2

Variegation and phase separation with about 5% rutile


This picture has its own page with more detail, click here to see it.

The glaze is a dolomite matte. G2571A, fired to cone 10R. High-fire reduction is among the best processes to exploit the variegating magic of rutile.

Links

Glossary Phase Separation
Phase separation in glaze melts creates microscopic discontinuities that affect transparency, color variegation, matte surfaces, and reactive glaze effects.
Glossary Crystalline glazes
A type of ceramic glaze made by potters. Giant multicolored crystals are grown on a super gloss low alumina high zinc glaze by controlling multiple holds and soaks during cooling in the kiln.
Glossary Crystallization
Ceramic glazes form crystals on cooling if the chemistry is right and the rate of cool is slow enough to permit molecular movement to the preferred orientation.
Glossary Opacifier
Glaze opacity refers to the degree to which it is opaque. Opacifiers are powders added to transparent ceramic glazes to make them opaque.
Glossary Reactive Glazes
In ceramics, reactive glazes have variegated surfaces that are a product of more melt fluidity and the presence of opacifiers, crystallizers and phase changers.
Glossary Reduction Firing
A method of firing stoneware where the kiln air intakes and burners are set to restrict or eliminate oxygen in the kiln such that metallic oxides convert to their reduced metallic state.
Glossary Magnesia Matte
Magnesia matte ceramic glazes are “microstructure mattes” while calcia mattes are “crystal mattes”. They have a micro-wrinkle surface that forms from a high viscosity melt and microscopic phase separation, both of which prevent levelling on freezi
Glossary Mechanism
Identifying the mechanism of a ceramic glaze recipe is the key to moving adjusting it, fixing it, reverse engineering it, even avoiding it!
Glossary Variegation
Ceramic glaze variegation refers to its visual character. This is an overview of the various mechanisms to make glazes dance with color, crystals, highlights, speckles, rivulets, etc.
Oxides MgO - Magnesium Oxide, Magnesia
Minerals Iron Pyrite
Iron pyrite, or Fool's Gold, is a common metallic mineral containing about 50% iron and 33% sulfur.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.