2019 Jiggering-Casting Project of Medalta 66 Mug
A cereal bowl jigger mold made using 3D printing
Beer Bottle Master Mold via 3D Printing
Better porosity for Brown Sugar Savers
Build a kiln monitoring device
Celebration Project
Coffee Mug Slip Casting Mold via 3D Printing
Comparing the Melt Fluidity of 16 Frits
Cookie Cutting clay with 3D printed cutters
Evaluating a clay's suitability for use in pottery
Make a mold for 4-gallon stackable calciners
Make Your Own Pyrometric Cones
Make your own sieve shaker to process ceramic slurries
Making a high quality ceramic tile
Making a Plaster Table
Making Bricks
Making our own kiln posts using a hand extruder
Medalta Ball Pitcher Slip Casting Mold via 3D Printing
Medalta Jug Master Mold Development
Mold Natches
Mother Nature's Porcelain - Plainsman 3B
Mug Handle Casting
Nursery plant pot mold via 3D printing
Pie-Crust Mug-Making Method
Plainsman 3D, Mother Nature's Porcelain/Stoneware
Pottery Classes
Project to Document a Shimpo Jiggering Attachment
Roll, Cut, Pull, Attach Handle-making Method
Seven reasons to do DIY underglazes
Slurry Mixing and Dewatering Your Own Clay Body
Testing a New Load of EP Kaolin
Using milk as a glaze
Videos of factory workers making holloware
Yixing Teapots

Medalta Jug Master Mold Development

I want to create a classic jug to commemorate those made by the Medalta Potteries here in the early part of the 20th century. I will use a casting process and 3D design and 3D printing for the mold making.

Related Information

Initial model drawing for a stoneware jug


This picture has its own page with more detail, click here to see it.

I found this picture online of one of the original jug styles they made. We are not including handle yet. We are learning (my Upwork worker Oleksii and I) about how to make these models more parameterized. This one has more than a dozen settings that I can change and the drawing adjusts automatically.


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy